Comparison of shear bond strength(SBS) between E-max ceramic and composite resin with two methods of cementation

نویسندگان

1 دانشگاه صنعتی خواجه نصیرالدین طوسی

2 دانشگاه فرهنگیان

3 دانشگاه علوم پزشکی مشهد

4 دانشگاه علوم پزشکی مشهد

doi
10.22088/cjdr.10.2.60
چکیده

Introduction: Today, the use of all-ceramic restorations has increased due to their physical properties as well as translucency and esthetic appearance . The aim of this study was to compare the shear bond strength (SBS) between two methods of e-max ceramic cementing . Materials & Methods: The study groups were 1 flowable composite as cement (FC group) and 2) choice2 cement (C2 group). The samples were fixed to a KOOPA universal testing machine for SBS testing. Tthe data were analyzed using SPSS 20 through T-test at significant level of P˂0.05. Results: The average SBS in the FC group was 10.41±2.17 and The average SBS in the C2 group was 13.28 ±1.52. There was a statistically significant difference between the SBS of both groups (p<0.001). Conclusion: This study demonstrated that ,the use of flowable composite instead of C2 cement is not recommended for cementing e-max ceramics.