Electrophoretic Deposition of Hydroxyapatite: Electrophoretic deposition of hydroxyapatite

نویسندگان

1 Materials and Energy Research Center, Tehran, Iran

2 Department of Biomedical Engineering, Islamic Azad University, Science and Research Branch,Tehran, Iran

3 Materials and Energy Research Center, Tehran, Iran

4 Materials and Energy Research Center, Tehran, Iran

5 Materials and Energy Research Center, Tehran, Iran

6 cCenter of Excellence in Electrochemistry, Faculty of Chemistry, University of Tehran, Tehran, Iran

doi
10.22037/ijps.v4.39820
چکیده

The purpose of this study was to investigate the deposition of the hydroxyapatite(HA) coating via the electrophoresis procedure. The HAdeposition was performedin an ethanol, methanol, acetone and isopropanol suspension. Methanol was foundto be the best deposition media. Among the different environmental conditions,including the encapsulation of the samples under two vacuum types of pressure(10-5-10-4and 2×10-2Torr) and also thepurge of the argon gas in the tube-likefurnace, the optimum environment was the one demonstrating the encapsulation underthe vacuum pressure of 2×10-2Torr (washing with argon gas of 99.9% purity). Afterthe examination of 3 sintering temperatures (1020, 1050 and 1100 ºC), the sinteringtemperature at 1050 ºC illustrated the most desired results. The samples sintered underthese conditions were apparently intact, most of the interfacial part of the coatingwas found to be attached to the substrate surface irregularities and no single crackswere observed.